Experimental Characterization of the Initial Shear Strength of Composite Masonry including AAC Blocks and DPC Layers
Martijn Vanheukelom,
Rajarshi Das,
Hervé Degée and
Bram Vandoren
Additional contact information
Martijn Vanheukelom: Construction Engineering Research Group, UHasselt–Hasselt University, Agoralaan, 3590 Diepenbeek, Belgium
Rajarshi Das: Construction Engineering Research Group, UHasselt–Hasselt University, Agoralaan, 3590 Diepenbeek, Belgium
Hervé Degée: Construction Engineering Research Group, UHasselt–Hasselt University, Agoralaan, 3590 Diepenbeek, Belgium
Bram Vandoren: Construction Engineering Research Group, UHasselt–Hasselt University, Agoralaan, 3590 Diepenbeek, Belgium
Sustainability, 2021, vol. 13, issue 22, 1-13
Abstract:
Modern masonry structures, apart from having a load-bearing function, are more and more subjected to additional non-structural requirements related to, e.g., thermal insulation and moisture control. This has respectively led to the introduction of thermal break layers, in practice often executed using autoclaved aerated concrete (AAC) blocks, and damp proof courses (DPC) in masonry walls. These modifications have an impact on the mechanical characteristics of the masonry, such as the shear strength. In this paper, an extensive experimental campaign is therefore conducted on masonry triplets to investigate the initial shear strength of concrete block and clay brick masonry, including AAC blocks. The impact of the the presence of a polyethylene DPC layer is also studied. Moreover, the position of the DPC membrane is varied, i.e., directly on top of the brick (which is generally not recommended yet common in construction practice) and in the middle of the mortar joint. In total, 138 shear tests were performed according to the EN 1052-3 standard, with low to moderate precompression levels. The test results focus on the differences in friction angle, shear modulus, and friction coefficient. It is concluded that the presence of an AAC block decreases the initial shear strength to a value which is lower than the one assumed by Eurocode 6. Moreover, when adding a DPC membrane, the shear strength is reduced even further to almost zero, in particular when the membrane is not put in the middle of the mortar joint.
Keywords: autoclaved aerated concrete (AAC); damp proof course (DPC); initial shear strength; EN 1052-3 (search for similar items in EconPapers)
JEL-codes: O13 Q Q0 Q2 Q3 Q5 Q56 (search for similar items in EconPapers)
Date: 2021
References: View complete reference list from CitEc
Citations:
Downloads: (external link)
https://www.mdpi.com/2071-1050/13/22/12749/pdf (application/pdf)
https://www.mdpi.com/2071-1050/13/22/12749/ (text/html)
Related works:
This item may be available elsewhere in EconPapers: Search for items with the same title.
Export reference: BibTeX
RIS (EndNote, ProCite, RefMan)
HTML/Text
Persistent link: https://EconPapers.repec.org/RePEc:gam:jsusta:v:13:y:2021:i:22:p:12749-:d:681839
Access Statistics for this article
Sustainability is currently edited by Ms. Alexandra Wu
More articles in Sustainability from MDPI
Bibliographic data for series maintained by MDPI Indexing Manager ().