Hydrolysis of Semi-finished Polyacrylonitrile (PAN) Fiber
Juan Xu and
Shulin An
Modern Applied Science, 2010, vol. 4, issue 11, 61
Abstract:
Based on above best preparation condition for semi-finished polyacrylonitrile (PAN) fiber via dry spinning at alkaline conditions, for example, hydrolyzing temperature keeps at 95?, the mass fraction of NaOH is 15%, water treatment is 60 min, the effect of bath ratio and the recycling of the bath on fiber water absorptivity were further investigated. Furthermore, the max recovery rate of the alkali solution was discussed. The results show that bath ratio has little effect on the water absorptivity of superabsorbent fiber obtained by hydrolyzing PAN precursor. The bath can be recycled at most three times, and maxmium recovery rate of the alkali solution is about 70%.
Date: 2010
References: View complete reference list from CitEc
Citations:
Downloads: (external link)
https://ccsenet.org/journal/index.php/mas/article/download/8038/6042 (application/pdf)
https://ccsenet.org/journal/index.php/mas/article/view/8038 (text/html)
Related works:
This item may be available elsewhere in EconPapers: Search for items with the same title.
Export reference: BibTeX
RIS (EndNote, ProCite, RefMan)
HTML/Text
Persistent link: https://EconPapers.repec.org/RePEc:ibn:masjnl:v:4:y:2010:i:11:p:61
Access Statistics for this article
More articles in Modern Applied Science from Canadian Center of Science and Education Contact information at EDIRC.
Bibliographic data for series maintained by Canadian Center of Science and Education ().