Correlation between Theoretical and Experimental Specific Surface Area Estimation for PANI and PANI (Zr) Composite
Tatiana N. Myasoedova,
Nina K. Plugotarenko,
Tatiana A. Moiseeva,
Eugeniy V. Vorobyev,
Vera V. Butova and
Viktor V. Petrov
Modern Applied Science, 2015, vol. 9, issue 13, 133
Abstract:
Polyaniline (PANI) and polyaniline/Zr (PANI/Zr) powders have been prepared by in situ polymerization method,and the morphology, structure and pore structure are investigated. Quantum-chemical calculations showed thatthe polyaniline structure formed with zirconium ions is not globular, but fiber-like, and its fiber patterns arecharacterized by clear orientation of individual fragments Estimation of the theoretical and experimental specificsurface area of the PANI/Zr composite is done. It is shown that the most preferred is the fiber-like structure withthe specific surface area about 128-162 m2/g, which stability may be improved by using zirconium (IV)containing substances as a dopant. Experimental specific surface area is 66.8 and 146.05 m2/g for PANI andPANI/Zr, respectively. Correlation between theoretical and experimental specific surface area PANI/Zrcomposite is observed.
Date: 2015
References: View complete reference list from CitEc
Citations:
Downloads: (external link)
https://ccsenet.org/journal/index.php/mas/article/download/51051/29705 (application/pdf)
https://ccsenet.org/journal/index.php/mas/article/view/51051 (text/html)
Related works:
This item may be available elsewhere in EconPapers: Search for items with the same title.
Export reference: BibTeX
RIS (EndNote, ProCite, RefMan)
HTML/Text
Persistent link: https://EconPapers.repec.org/RePEc:ibn:masjnl:v:9:y:2015:i:13:p:133
Access Statistics for this article
More articles in Modern Applied Science from Canadian Center of Science and Education Contact information at EDIRC.
Bibliographic data for series maintained by Canadian Center of Science and Education ().