Li+-migration influencing factors and non-destructive life extension of quasi-solid-state polymer electrolytes
Peiying Li,
Jinjin Hao,
Shuang He,
Zenghua Chang,
Xiaolei Li,
Rennian Wang,
Wen Ma,
Jiantao Wang,
Yuhao Lu,
Hong Li,
Liqun Zhang and
Weidong Zhou ()
Additional contact information
Peiying Li: Beijing University of Chemical Technology
Jinjin Hao: Beijing University of Chemical Technology
Shuang He: Beijing University of Chemical Technology
Zenghua Chang: China Automotive Battery Research Institute Co. Ltd. Beijing
Xiaolei Li: Beijing University of Chemical Technology
Rennian Wang: China Automotive Battery Research Institute Co. Ltd. Beijing
Wen Ma: Key Laboratory of Consumer Lithium-Ion Battery in Fujian
Jiantao Wang: China Automotive Battery Research Institute Co. Ltd. Beijing
Yuhao Lu: Key Laboratory of Consumer Lithium-Ion Battery in Fujian
Hong Li: Chinese Academy of Sciences
Liqun Zhang: Beijing University of Chemical Technology
Weidong Zhou: Beijing University of Chemical Technology
Nature Communications, 2025, vol. 16, issue 1, 1-14
Abstract:
Abstract Polymer-based quasi-solid-state electrolytes (QSSE) are believed to be the most feasible candidates for solid-state batteries, but they are hindered by relatively lower ionic conductivity and narrower electrochemical window. Here, we synthesize a series of ether-free acrylates containing Li+-ligands for high-voltage-stable QSSEs. Our findings demonstrate that the polymer-involved solvation structure is critical in determining the ionic conductivity, and low-temperature crystallization of the polymer can be used for non-destructive life extension of batteries. The prepared polymers do not contain ether unit and exhibit a polymerization degree of 99% in cells without residual double-bonded monomer, endowing them with high antioxidation capability and compatibility with high-voltage positive electrodes including LiNi0.85Co0.075Mn0.075O2, 4.6 V LiCoO2 and 4.8 V Li1.13Ni0.3Mn0.57O2. The confinement of liquid in QSSEs effectively suppresses the interfacial reactions, but the residual interface reactions still gradually consume liquid electrolytes and cause capacity fading, due to the limited diffusion of the confined solvent to wet the interface. Through crystallizing the polymer matrices at −50 °C, the confined liquid in QSSEs is released and re-wets the Li-metal/polymer interface, thereby recovering the capacity and extending the life of solid-state batteries in a non-destructive manner.
Date: 2025
References: View references in EconPapers View complete reference list from CitEc
Citations:
Downloads: (external link)
https://www.nature.com/articles/s41467-025-59020-w Abstract (text/html)
Related works:
This item may be available elsewhere in EconPapers: Search for items with the same title.
Export reference: BibTeX
RIS (EndNote, ProCite, RefMan)
HTML/Text
Persistent link: https://EconPapers.repec.org/RePEc:nat:natcom:v:16:y:2025:i:1:d:10.1038_s41467-025-59020-w
Ordering information: This journal article can be ordered from
https://www.nature.com/ncomms/
DOI: 10.1038/s41467-025-59020-w
Access Statistics for this article
Nature Communications is currently edited by Nathalie Le Bot, Enda Bergin and Fiona Gillespie
More articles in Nature Communications from Nature
Bibliographic data for series maintained by Sonal Shukla () and Springer Nature Abstracting and Indexing ().