Abstract:
Self-consolidating concrete (SCC) has been successfully employed to reduce construction time and enhance the quality, performance, and esthetic appearance of concrete structures. This research aimed at developing environmentally friendly fiber-reinforced concrete (FRC) consisting of SCC and recycled polypropylene (PP) fibers for sustainable construction of city buildings and transportation infrastructure. The addition of the PP fibers to SCC helps reducing shrinkage cracks and providing enhanced mechanical properties, durability, and ductility of the concrete materials. Several mix designs of self-consolidating fiber-reinforced concrete (SCFRC) were experimentally examined. Material and esthetic properties of the SCFRC mixtures that include micro silica, fly ash, and PP fibers were evaluated. Trial-and-adjustment method was employed to obtain practically optimum SCFRC mixtures, mixtures that are affordable and easy to make possessing enhanced compressive strength and esthetic properties. Slump flow and air content testing methods were used to determine the fresh properties of the SCFRC mixtures, and the esthetic properties of the mixtures were also evaluated. The hardened properties of the SCFRC mixtures were examined using three- and seven-day compression tests. The amount of fine/coarse aggregate, water, and other admixtures were varied while the Portland cement content in all mixtures was maintained unchanged. The maximum three-day compressive strength was 43.17 MPa and the largest slump flow was 736.6 mm. Test results showed enhanced material properties such as slump flow, air content and compressive strength values of the SCFRC mixtures and their excellent esthetic appearance. The favorable seven-day compressive strength of the SCFRC mixture, with 4.8 percent air content and 660.4 mm slump flow, is 39.26 MPa. The mixtures' in this study are proven to be advantageous for potential SCFRC applications in architectural structures including building façades and esthetically-pleasing bridges.
Keywords: self-consolidating concrete (SCC); fiber-reinforced concrete (FRC); mix designs; enhanced material properties; esthetic appearance (search for similar items in EconPapers)
JEL-codes: Q56 (search for similar items in EconPapers)
References: Add references at CitEc
Citations:
Downloads: (external link)
https://www.intechopen.com/chapters/74421 (text/html)
Related works:
This item may be available elsewhere in EconPapers: Search for items with the same title.
Export reference: BibTeX
RIS (EndNote, ProCite, RefMan)
HTML/Text
Persistent link: https://EconPapers.repec.org/RePEc:ito:pchaps:222263
DOI: 10.5772/intechopen.95091
Access Statistics for this chapter
More chapters in Chapters from IntechOpen
Bibliographic data for series maintained by Slobodan Momcilovic ().