Experimental and modeling analysis of thermal runaway propagation over the large format energy storage battery module with Li4Ti5O12 anode

Peifeng Huang, Ping Ping, Ke Li, Haodong Chen, Qingsong Wang, Jennifer Wen and Jinhua Sun

Applied Energy, 2016, vol. 183, issue C, 659-673

Abstract: Insight of the thermal characteristics and potential flame spread over lithium-ion battery (LIB) modules is important for designing battery thermal management system and fire protection measures. Such thermal characteristics and potential flame spread are also dependent on the different anode and cathode materials as well as the electrolyte. In the present study, thermal behavior and flame propagation over seven 50Ah Li(Ni1/3Mn1/3Co1/3)O2/Li4Ti5O12 large format LIBs arranged in rhombus and parallel layouts were investigated by directly heating one of the battery units. Such batteries have already been used commercially for energy storage while relatively little is known about its safety features in connection with potential runaway caused fire and explosion hazards. It was found in the present heating tests that fire-impingement resulted in elevated temperatures in the immediate vicinity of the LIBs that were in the range of between 200°C and 900°C. Such temperature aggravated thermal runaway (TR) propagation, resulting in rapid temperature rise within the battery module and even explosions after 20min of “smoldering period”. The thermal runaway and subsequent fire and explosion observed in the heating test was attributed to the violent reduction of the cathode material which coexisted with the electrolyte when the temperature exceeded 260°C. Separate laboratory tests, which measured the heat and gases generation from samples of the anode and cathode materials using C80 calorimeter, provided insight of the physical-chemistry processes inside the battery when the temperature reaches between 30°C and 300°C. The self-accelerating decomposition temperature of the cell, regarded as the critical temperature to trigger TR propagation, was calculated as 126.1 and 139.2°C using the classical Semenov and Frank-Kamenetskii models and the measurements of the calorimeter with the samples. These are consistent with the measured values in the heating tests in which TR propagated. The events leading to the explosions in the test for the rhombus layout was further analyzed and two possible explanations were postulated and analyzed based on either internal catalytic reactions or Boiling Liquid Expansion Vapor Explosion (BLEVE).

Keywords: Lithium ion battery safety; Thermal runaway propagation; Self-accelerating reaction temperature; Semenov and Frank-Kamenetskii models; Catalytic reactions and BLEVE (search for similar items in EconPapers)
Date: 2016
References: View references in EconPapers View complete reference list from CitEc
Citations: View citations in EconPapers (22)

Downloads: (external link)
http://www.sciencedirect.com/science/article/pii/S0306261916312697
Full text for ScienceDirect subscribers only

Related works:
This item may be available elsewhere in EconPapers: Search for items with the same title.

Export reference: BibTeX RIS (EndNote, ProCite, RefMan) HTML/Text

Persistent link: https://EconPapers.repec.org/RePEc:eee:appene:v:183:y:2016:i:c:p:659-673

Ordering information: This journal article can be ordered from
http://www.elsevier.com/wps/find/journaldescription.cws_home/405891/bibliographic
http://www.elsevier. ... 405891/bibliographic

DOI: 10.1016/j.apenergy.2016.08.160

Access Statistics for this article

Applied Energy is currently edited by J. Yan

More articles in Applied Energy from Elsevier
Bibliographic data for series maintained by Catherine Liu ().

 
Page updated 2025-03-19
Handle: RePEc:eee:appene:v:183:y:2016:i:c:p:659-673